Temperatura de fusión: 945 °C

Quick Comparison

Tin Bronze

ASTM B505 Grade C90700

Suministrada por:

1 proveedor Matmatch

Leaded Tin Bronze

ASTM B505 Grade C92700

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95200

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95520

Suministrada por:

1 proveedor Matmatch

Bronce fosforado

JIS C5210HQ Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Bronce fosforado

JIS C5240HQ Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Wrought Copper Brass Yellow Brass

EN 1652 Grade CuZn40 R340

Bronce fosforado

JIS C5191HQ Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Bronce fosforado

JIS C5210 Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Bronce fosforado

JIS C5240 Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Wrought Copper Nickel Silver Grade

BS NS101 Nickel Silver

Wrought Copper Brass Yellow Brass

EN 1652 Grade CuZn10 O60

Wrought Copper Brass Yellow Brass

EN 1652 Grade CuZn30 O60

Wrought Copper Brass Yellow Brass

EN 12166 Grade CuZn36 O60

Wrought Copper Brass Yellow Brass

EN 12164 Grade CuZn40 R400
Página 1 de 176