Límite elástico Rp 0,2: 620 - 725 MPa

Quick Comparison

Acero bajo en carbono

EN 10083-3 Grade 20MnB5 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Unclassified Low Alloy Steel

EN 10025-6 Grade S690QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10028-6 Grade P690QH quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

7000 Serie

AA Standards Grade 7075 T6

Suministrada por:

3 proveedores de Matmatch

7000 Serie

AA Standards Grade 7075 T651

Suministrada por:

3 proveedores de Matmatch

Acero inoxidable endurecido por precipitación

UGIMA® 4542 +P930/H1150

Suministrada por:

Ugitech

Chromium Molybdenum Steel

ASTM A542 Type A Class 2 Quenched and Tempered

Suministrada por:

1 proveedor Matmatch

Chromium Molybdenum Steel

ASTM A542 Type D Class 1 Quenched and Tempered

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TF00

Nickel Chromium Iron Alloy

VDM® Alloy 718

Suministrada por:

VDM Metals

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TF00

Wrought Copper High Copper Alloy

ASTM B643 Grade C17200 TH04

Wrought Copper High Copper Alloy

ASTM B534 Grade C17500 TF00

Wrought Copper High Copper Alloy

ASTM B441 Grade C17500 TH04
Página 1 de 25