DIN 1.3820

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

typical value

Dimension

PropertyValueComment

Thickness

200 mm

Show Material materials with Thickness of 200 mm

max.

Mechanical

PropertyTemperatureValueComment

Charpy impact energy

23.0 °C

180 J

Show Material materials with Charpy impact energy of 180 J

min.

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

typical value

Elongation

23.0 °C

40 %

Show Material materials with Elongation of 40 %

min., A5.65

Hardness, Vickers

23.0 °C

270 - 300 [-]

Show Material materials with Hardness, Vickers of 270 - 300 [-]

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

typical value

Tensile strength

23.0 °C

900 - 1050 MPa

Show Material materials with Tensile strength of 900 - 1050 MPa

Yield strength

23.0 °C

600 - 800 MPa

Show Material materials with Yield strength of 600 - 800 MPa

Chemical properties

PropertyValueComment

Carbon

0.12 %

Show Material materials with Carbon of 0.12 %

max.

Chromium

18 - 20 %

Show Material materials with Chromium of 18 - 20 %

max.

Iron

Balance

Manganese

9 - 11 %

Show Material materials with Manganese of 9 - 11 %

Molybdenum

1 %

Show Material materials with Molybdenum of 1 %

max.

Nickel

1 %

Show Material materials with Nickel of 1 %

max.

Nitrogen

0.4 - 0.65 %

Show Material materials with Nitrogen of 0.4 - 0.65 %

max

Phosphorus

0.06 %

Show Material materials with Phosphorus of 0.06 %

max.

Silicon

1 %

Show Material materials with Silicon of 1 %

max.

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

max.