DIN EN 10085 Grade 1.8522

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

typical value

Dimension

PropertyValue

Thickness

16 - 250 mm

Show Material materials with Thickness of 16 - 250 mm

Mechanical

PropertyTemperatureValueComment

Charpy impact energy

23.0 °C

30 - 45 J

Show Material materials with Charpy impact energy of 30 - 45 J

min.

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

typical value

Elongation

23.0 °C

11 - 13 %

Show Material materials with Elongation of 11 - 13 %

min., A5.65

Hardness, Brinell

23.0 °C

248 [-]

Show Material materials with Hardness, Brinell of 248 [-]

max.

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

typical value

Tensile strength

23.0 °C

900 - 1350 MPa

Show Material materials with Tensile strength of 900 - 1350 MPa

Yield strength

23.0 °C

700 - 950 MPa

Show Material materials with Yield strength of 700 - 950 MPa

min.

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K

typical value

Specific heat capacity

23.0 °C

470 J/(kg·K)

Show Material materials with Specific heat capacity of 470 J/(kg·K)

typical value

Thermal conductivity

23.0 °C

39 W/(m·K)

Show Material materials with Thermal conductivity of 39 W/(m·K)

typical value

Electrical

PropertyValueComment

Specific Electrical conductivity

7.8 % IACS

Show Material materials with Specific Electrical conductivity of 7.8 % IACS

typical value

Chemical properties

PropertyValueComment

Carbon

0.29 - 0.36 %

Show Material materials with Carbon of 0.29 - 0.36 %

Chromium

2.8 - 3.3 %

Show Material materials with Chromium of 2.8 - 3.3 %

Copper

0.1 %

Show Material materials with Copper of 0.1 %

max. DIN EN ISO 683-17: 0.1-0.4

Iron

Balance

Manganese

0.4 - 0.7 %

Show Material materials with Manganese of 0.4 - 0.7 %

Molybdenum

0.7 - 1 %

Show Material materials with Molybdenum of 0.7 - 1 %

DIN EN ISO 683-17: 0.7-1.2

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

max. DIN EN ISO 683-17

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

max.

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

max. DIN EN ISO 683-17: 0.1-0.4

Sulfur

0.035 %

Show Material materials with Sulfur of 0.035 %

max. DIN EN ISO 683-17: 0.015

Vanadium

0.15 - 0.25 %

Show Material materials with Vanadium of 0.15 - 0.25 %