DIN 1.5223 Quenched and Tempered

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

typical value

Dimension

PropertyValue

Thickness

16 - 100 mm

Show Material materials with Thickness of 16 - 100 mm

Mechanical

PropertyTemperatureValueComment

Charpy impact energy

23.0 °C

15 - 30 J

Show Material materials with Charpy impact energy of 15 - 30 J

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

typical value

Elongation

23.0 °C

10 - 12 %

Show Material materials with Elongation of 10 - 12 %

min., A5.65

Hardness, Brinell

23.0 °C

217 [-]

Show Material materials with Hardness, Brinell of 217 [-]

max. in soft annealed condition

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

typical value

Reduction of area

23.0 °C

30 - 40 %

Show Material materials with Reduction of area of 30 - 40 %

min.

Tensile strength

23.0 °C

880 - 1270 MPa

Show Material materials with Tensile strength of 880 - 1270 MPa

Yield strength

23.0 °C

685 - 885 MPa

Show Material materials with Yield strength of 685 - 885 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.33E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.33E-5 1/K

Typical for Manganese Steel

Melting point

1382 - 1529 °C

Show Material materials with Melting point of 1382 - 1529 °C

Typical for Manganese Steel

Specific heat capacity

23.0 °C

510 - 553 J/(kg·K)

Show Material materials with Specific heat capacity of 510 - 553 J/(kg·K)

Typical for Manganese Steel

Thermal conductivity

23.0 °C

14 - 16 W/(m·K)

Show Material materials with Thermal conductivity of 14 - 16 W/(m·K)

Typical for Manganese Steel

Chemical properties

PropertyValueComment

Carbon

0.38 - 0.45 %

Show Material materials with Carbon of 0.38 - 0.45 %

Iron

Balance

Manganese

1.6 - 1.9 %

Show Material materials with Manganese of 1.6 - 1.9 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

max.

Silicon

0.15 - 0.35 %

Show Material materials with Silicon of 0.15 - 0.35 %

Sulfur

0.035 %

Show Material materials with Sulfur of 0.035 %

max.

Vanadium

0.07 - 0.12 %

Show Material materials with Vanadium of 0.07 - 0.12 %