DEFSTAN 95-14 Grade S144

Want to keep this datasheet? Save it now in your required format

Description

3S144 is a British aerospace grade, precipitation hardenable stainless steel. It is widely used in the aerospace industry benefiting from a combination of strength and moderate corrosion resistance. BS S143 and BS S145 are chemically identical. S144 is supplied in bar form with heat treatment applied.

Related Standards

This material data has been provided by Righton Blackburns,Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

7.9 - 8.2 g/cm³

Show Material materials with Density of 7.9 - 8.2 g/cm³

Typical for Austenitic Stainless Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

195 GPa

Show Material materials with Elastic modulus of 195 GPa

Typical for Austenitic Stainless Steel

Elongation A50

20.0 °C

12 %

Show Material materials with Elongation A50 of 12 %

Hardness, Brinell

20.0 °C

341 [-]

Show Material materials with Hardness, Brinell of 341 [-]

Poisson's ratio

20.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Austenitic Stainless Steel

Shear modulus

20.0 °C

77 GPa

Show Material materials with Shear modulus of 77 GPa

Typical for Austenitic Stainless Steel

Tensile strength

20.0 °C

1130 - 1330 MPa

Show Material materials with Tensile strength of 1130 - 1330 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

1.7E-5 - 1.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K

Typical for Austenitic Stainless Steel

Melting point

1375 - 1450 °C

Show Material materials with Melting point of 1375 - 1450 °C

Typical for Austenitic Stainless Steel

Specific heat capacity

20.0 °C

440 J/(kg·K)

Show Material materials with Specific heat capacity of 440 J/(kg·K)

Typical for Austenitic Stainless Steel

Thermal conductivity

20.0 °C

11 - 21 W/(m·K)

Show Material materials with Thermal conductivity of 11 - 21 W/(m·K)

Typical for Austenitic Stainless Steel

Electrical

PropertyTemperatureValueComment

Electrical resistivity

20.0 °C

8.5E-7 Ω·m

Show Material materials with Electrical resistivity of 8.5E-7 Ω·m

Typical for Austenitic Stainless Steel

Chemical properties

PropertyValue

Carbon

0.08 %

Show Material materials with Carbon of 0.08 %

Chromium

Balance

Copper

1.2 - 2 %

Show Material materials with Copper of 1.2 - 2 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Molybdenum

1.2 - 2 %

Show Material materials with Molybdenum of 1.2 - 2 %

Nickel

5 - 5.8 %

Show Material materials with Nickel of 5 - 5.8 %

Niobium

0.1 - 0.4 %

Show Material materials with Niobium of 0.1 - 0.4 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.6 %

Show Material materials with Silicon of 0.6 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %