S32750 Stainless Steel

View suppliers (67)
Want to keep this datasheet? Save it now in your required format

Description

1.4410 (X2CrNiMoN25-7-4) is the standard grade of super-duplex stainless steel based on 25% chromium, 7% nickel and significant additions of molybdenum, manganese and nitrogen. It shows the following features and properties:


  • Very high strength
  • Very good resistance to pitting and crevice corrosion
  • Excellent resistance to chloride stress corrosion cracking
  • Good workability and weldability
  • Related Standards

    Equivalent Materials

    This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Mechanical

    PropertyTemperatureValueComment

    Elongation

    23.0 °C

    15 %

    Show Material materials with Elongation of 15 %

    Hardness, Brinell

    23.0 °C

    280 [-]

    Show Material materials with Hardness, Brinell of 280 [-]

    max.

    Tensile strength

    23.0 °C

    760 - 800 MPa

    Show Material materials with Tensile strength of 760 - 800 MPa

    Yield strength

    23.0 °C

    315 - 550 MPa

    Show Material materials with Yield strength of 315 - 550 MPa

    Chemical properties

    PropertyValue

    Chromium

    25 %

    Show Material materials with Chromium of 25 %

    Iron

    Balance

    Molybdenum

    4 %

    Show Material materials with Molybdenum of 4 %

    Nickel

    7 %

    Show Material materials with Nickel of 7 %

    Nitrogen

    0.28 %

    Show Material materials with Nitrogen of 0.28 %

    Technological properties

    Property
    Application areas

    Offshore & marine: Offshore platforms and equipment, components for gas, oil and process cooling plants, wellhead and subsea wellhead fittings, desalination plants, seawater cooled heat exchangers and high strength fasteners;Chemical processing: Chemical tanks, flue gas filters, acid distillation components and heat exchangers

    Corrosion properties

    Very good corrosion resistance

    General machinability

    Good workability