Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 23.0 °C | 12 % Show Material materials with Elongation of 12 % |
Hardness, Brinell | 23.0 °C | 255 - 321 [-] Show Material materials with Hardness, Brinell of 255 - 321 [-] |
Tensile strength | 23.0 °C | 880 - 1080 MPa Show Material materials with Tensile strength of 880 - 1080 MPa |
Yield strength | 23.0 °C | 690 MPa Show Material materials with Yield strength of 690 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbon | 0.16 % Show Material materials with Carbon of 0.16 % | max. | |
Chromium | 16.5 % Show Material materials with Chromium of 16.5 % | ||
Iron | Balance | ||
Manganese | 0.3 % Show Material materials with Manganese of 0.3 % | ||
Nickel | 2.5 % Show Material materials with Nickel of 2.5 % | ||
Silicon | 0.25 % Show Material materials with Silicon of 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: High strength fasteners, bolts and shafts;Aerospace: Various aerospace components including high strength fasteners;Other: Compressor forms, dairies, machine tool industry, marine engineering, paper mills, plant engineering, starch mills and yeast factories | |
Corrosion properties | Excellent corrosion resistance |