S130 Stainless Steel

View suppliers (46)
Want to keep this datasheet? Save it now in your required format

Description

1.4550 (X6CrNiNb1810) is an austenitic grade of stainless steel stabilised with niobium to prevent carbide precipitation and inter-granular corrosion, especially in welded fabrications. It resists oxidation and scaling and is used up to 900°C for aerospace applications including aircraft exhaust manifolds and other elevated temperature applications. The weldability of S130 is excellent, and with no post-weld heat treatment required it is particularly suitable for welded structures. It shows the following features and properties:


  • High strength and toughness
  • Good oxidation resistance up to 900°C
  • High corrosion resistance
  • Related Standards

    Equivalent Materials

    This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Mechanical

    PropertyTemperatureValue

    Elongation

    23.0 °C

    35 %

    Show Material materials with Elongation of 35 %

    Hardness, Brinell

    23.0 °C

    140 - 220 [-]

    Show Material materials with Hardness, Brinell of 140 - 220 [-]

    Tensile strength

    23.0 °C

    540 MPa

    Show Material materials with Tensile strength of 540 MPa

    Yield strength

    23.0 °C

    210 MPa

    Show Material materials with Yield strength of 210 MPa

    Chemical properties

    PropertyValueComment

    Carbon

    0.08 %

    Show Material materials with Carbon of 0.08 %

    max.

    Chromium

    18 %

    Show Material materials with Chromium of 18 %

    Iron

    Balance

    Manganese

    1 %

    Show Material materials with Manganese of 1 %

    Molybdenum

    1 %

    Show Material materials with Molybdenum of 1 %

    max.

    Nickel

    9 %

    Show Material materials with Nickel of 9 %

    Niobium

    1.1 %

    Show Material materials with Niobium of 1.1 %

    max.

    Technological properties

    Property
    Application areas

    Aerospace: Aerospace components and fasteners;Other: Breweries, cellulose, industry, dairies, fermentation industry, food processing, leather industry, machine tool industries, nitric acid plants, nuclear engineering, paper mills and production of explosives

    Cold Forming

    Good cold working characteristics

    Corrosion properties

    High corrosion resistance

    Looking for suppliers of this material? Click to see 46 supplier of S130 Stainless Steel on Matmatch