powercore® C 120-23

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTemperature

Density

7.65 g/cm³

Show Material materials with Density of 7.65 g/cm³ at 23.0 °C

23.0 °C

Grain structure

Grain oriented electrical steel

Dimension

PropertyValue

Thickness

0.23 mm

Show Material materials with Thickness of 0.23 mm

Mechanical

PropertyValueTemperatureComment

Elongation A80

6 - 14 %

Show Material materials with Elongation A80 of 6 - 14 % at 23.0 °C

23.0 °C

Elongation A80, transverse

24 - 48 %

Show Material materials with Elongation A80, transverse of 24 - 48 % at 23.0 °C

23.0 °C

Hardness, Rockwell B

75 - 85 [-]

Show Material materials with Hardness, Rockwell B of 75 - 85 [-] at 23.0 °C

23.0 °C

15T

Hardness, Vickers, 0.1

175 - 195 [-]

Show Material materials with Hardness, Vickers, 0.1 of 175 - 195 [-] at 23.0 °C

23.0 °C

Tensile strength

330 - 370 MPa

Show Material materials with Tensile strength of 330 - 370 MPa at 23.0 °C

23.0 °C

Tensile strength, transverse

390 - 420 MPa

Show Material materials with Tensile strength, transverse of 390 - 420 MPa at 23.0 °C

23.0 °C

Yield strength Rp0.2

300 - 340 MPa

Show Material materials with Yield strength Rp0.2 of 300 - 340 MPa at 23.0 °C

23.0 °C

Yield strength Rp0.2, transverse

330 - 360 MPa

Show Material materials with Yield strength Rp0.2, transverse of 330 - 360 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueComment

Max service temperature

840 °C

Show Material materials with Max service temperature of 840 °C

according to DIN IEC 60404-12, under inert gas for 2 h

Electrical

PropertyValueTemperatureComment

Electrical resistivity

4.8E-7 Ω·m

Show Material materials with Electrical resistivity of 4.8E-7 Ω·m at 23.0 °C

23.0 °C

Surface insulation resistance

10 Ω·cm²

Show Material materials with Surface insulation resistance of 10 Ω·cm² at 23.0 °C

23.0 °C

according to DIN IEC 60404-11

Magnetic

PropertyValueTemperatureComment

Coercive force

5 A/m

Show Material materials with Coercive force of 5 A/m at 23.0 °C

23.0 °C

Curie temperature

745 °C

Show Material materials with Curie temperature of 745 °C

Guaranteed core loss

1.2 [-]

Show Material materials with Guaranteed core loss of 1.2 [-] at 23.0 °C

23.0 °C

at 1.7 T and 50 Hz

Guaranteed polarization

1.78 [-]

Show Material materials with Guaranteed polarization of 1.78 [-] at 23.0 °C

23.0 °C

at 800 A/m

Saturation polarization

2.03 T

Show Material materials with Saturation polarization of 2.03 T at 23.0 °C

23.0 °C

Typical core loss

1.18 [-]

Show Material materials with Typical core loss of 1.18 [-] at 23.0 °C

23.0 °C

at 1.7 T and 50 Hz

Typical polarization

1.83 [-]

Show Material materials with Typical polarization of 1.83 [-] at 23.0 °C

23.0 °C

at 800 A/m

Technological properties

Property
Application areas

Large power transformers, distribution transformers, small transformers, current transformers, shunt reactors, wound cores, power generators

Coating

Both sides coated, coating thickness: 2 µm - 5 µm

Other

Advantages of powercore®: Energy efficiency thanks to minimal losses at full load and reduced no-load losses, reduced noise emission thanks to minimized magnetostriction and improved insulation properties, cost benefits thanks to lower core weights and more compact dimensions.