General

Density

ρ

7.65 g/cm³ at 20 °C

Grain structure

Grain oriented electrical steel

Dimension

Thickness

t

0.27 mm

Mechanical

Elongation A80

A80

6 - 14 % at 20 °C

Show Silicon Steel materials with Elongation A80 of 6 - 14 % at 20 °C

Elongation A80, transverse

A80,trans

24 - 48 % at 20 °C

Show Silicon Steel materials with Elongation A80, transverse of 24 - 48 % at 20 °C

Hardness, Rockwell B

HRB

75 - 85 [-] at 20 °C

Show Silicon Steel materials with Hardness, Rockwell B of 75 - 85 [-] at 20 °C

15T

Hardness, Vickers, 0.1

HV 0.1

175 - 195 [-] at 20 °C

Show Silicon Steel materials with Hardness, Vickers, 0.1 of 175 - 195 [-] at 20 °C

Tensile strength

Rm

330 - 370 MPa at 20 °C

Show Silicon Steel materials with Tensile strength of 330 - 370 MPa at 20 °C

Tensile strength, transverse

Rm,trans

390 - 420 MPa at 20 °C

Show Silicon Steel materials with Tensile strength, transverse of 390 - 420 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

300 - 340 MPa at 20 °C

Show Silicon Steel materials with Yield strength Rp0.2 of 300 - 340 MPa at 20 °C

Yield strength Rp0.2, transverse

Rp0.2,trans

330 - 360 MPa at 20 °C

Show Silicon Steel materials with Yield strength Rp0.2, transverse of 330 - 360 MPa at 20 °C

Thermal

Max service temperature

Tmax

840 °C

according to DIN IEC 60404-12, under inert gas for 2 h

Electrical

Electrical resistivity

ρel

4.8E-7 Ω·m at 20 °C

Surface insulation resistance

SIR

10 Ω·cm² at 20 °C

according to DIN IEC 60404-11

Magnetic

Coercive force

Hc

5 A/m at 20 °C

Curie temperature

Tc

745 °C

Guaranteed core loss

Clossguar

0.95 [-] at 20 °C

at 1.7 T and 50 Hz

Guaranteed polarization

Jguar

1.88 [-] at 20 °C

at 800 A/m

Saturation polarization

Js

2.03 T at 20 °C

Typical core loss

Closstyp

0.93 [-] at 20 °C

at 1.7 T and 50 Hz

Typical polarization

Jtyp

1.91 [-] at 20 °C

at 800 A/m

Technological properties

Application areas

Large power transformers, distribution transformers, small transformers, current transformers, shunt reactors, wound cores, power generators

Coating

Both sides coated, coating thickness: 2 µm - 5 µm

Other

Advantages of powercore®: Energy efficiency thanks to minimal losses at full load and reduced no-load losses, reduced noise emission thanks to minimized magnetostriction and improved insulation properties, cost benefits thanks to lower core weights and more compact dimensions.

This material data has been provided by Matmatch.