powercore® H 110-30

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.65 g/cm³

Show Material materials with Density of 7.65 g/cm³

Grain structure

Grain oriented electrical steel

Dimension

PropertyValue

Thickness

0.3 mm

Show Material materials with Thickness of 0.3 mm

Mechanical

PropertyTemperatureValueComment

Elongation A80

23.0 °C

6 - 14 %

Show Material materials with Elongation A80 of 6 - 14 %

Elongation A80, transverse

23.0 °C

24 - 48 %

Show Material materials with Elongation A80, transverse of 24 - 48 %

Hardness, Rockwell B

23.0 °C

75 - 85 [-]

Show Material materials with Hardness, Rockwell B of 75 - 85 [-]

15T

Hardness, Vickers, 0.1

23.0 °C

175 - 195 [-]

Show Material materials with Hardness, Vickers, 0.1 of 175 - 195 [-]

Tensile strength

23.0 °C

330 - 370 MPa

Show Material materials with Tensile strength of 330 - 370 MPa

Tensile strength, transverse

23.0 °C

390 - 420 MPa

Show Material materials with Tensile strength, transverse of 390 - 420 MPa

Yield strength Rp0.2

23.0 °C

300 - 340 MPa

Show Material materials with Yield strength Rp0.2 of 300 - 340 MPa

Yield strength Rp0.2, transverse

23.0 °C

330 - 360 MPa

Show Material materials with Yield strength Rp0.2, transverse of 330 - 360 MPa

Thermal

PropertyValueComment

Max service temperature

840 °C

Show Material materials with Max service temperature of 840 °C

according to DIN IEC 60404-12, under inert gas for 2 h

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

4.8E-7 Ω·m

Show Material materials with Electrical resistivity of 4.8E-7 Ω·m

Surface insulation resistance

23.0 °C

10 Ω·cm²

Show Material materials with Surface insulation resistance of 10 Ω·cm²

according to DIN IEC 60404-11

Magnetic

PropertyTemperatureValueComment

Coercive force

23.0 °C

5 A/m

Show Material materials with Coercive force of 5 A/m

Curie temperature

745 °C

Show Material materials with Curie temperature of 745 °C

Guaranteed core loss

23.0 °C

1.1 [-]

Show Material materials with Guaranteed core loss of 1.1 [-]

at 1.7 T and 50 Hz

Guaranteed polarization

23.0 °C

1.88 [-]

Show Material materials with Guaranteed polarization of 1.88 [-]

at 800 A/m

Saturation polarization

23.0 °C

2.03 T

Show Material materials with Saturation polarization of 2.03 T

Typical core loss

23.0 °C

1.08 [-]

Show Material materials with Typical core loss of 1.08 [-]

at 1.7 T and 50 Hz

Typical polarization

23.0 °C

1.9 [-]

Show Material materials with Typical polarization of 1.9 [-]

at 800 A/m

Technological properties

Property
Application areas

Large power transformers, distribution transformers, small transformers, current transformers, shunt reactors, wound cores, power generators

Coating

Both sides coated, coating thickness: 2 µm - 5 µm

Other

Advantages of powercore®: Energy efficiency thanks to minimal losses at full load and reduced no-load losses, reduced noise emission thanks to minimized magnetostriction and improved insulation properties, cost benefits thanks to lower core weights and more compact dimensions.