General
Property | Value |
---|---|
Density | 1.38 - 1.4 g/cm³ Show Material materials with Density of 1.38 - 1.4 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 2.2 - 3.3 GPa Show Material materials with Elastic modulus of 2.2 - 3.3 GPa | |
Elongation | 10.0 - 60.0 % Show Material materials with Elongation of 10.0 - 60.0 % | |
Impact strength, Charpy notched | 2.0 - 50.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 2.0 - 50.0 kJ/m² | |
Impact strength, Charpy unnotched | 20 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 20 kJ/m² | |
Tensile strength | 30.0 - 60.0 MPa Show Material materials with Tensile strength of 30.0 - 60.0 MPa | at 4-6% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 6e-05 - 8e-05 1/K Show Material materials with Coefficient of thermal expansion of 6e-05 - 8e-05 1/K |
Specific heat capacity | 850.0 - 900.0 J/(kg·K) Show Material materials with Specific heat capacity of 850.0 - 900.0 J/(kg·K) |
Thermal conductivity | 0.14 - 0.17 W/(m·K) Show Material materials with Thermal conductivity of 0.14 - 0.17 W/(m·K) |
Flammability | UL 94 V0 |
Electrical
Property | Value |
---|---|
Dielectric constant | 3.5 [-] Show Material materials with Dielectric constant of 3.5 [-] |
Electrical resistivity | 10000000000000 Ω·m Show Material materials with Electrical resistivity of 10000000000000 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Pipes, window profiles, furniture | |
Processing methods | Injection molding, blow molding, extrusion, thermoforming |