Copolyamide based on epsilon-caprolactam, hexamethylenediamine and terephthalic acid Reinforced with 50% Glass Fibers (PA6/6T+GF50)

Alternative and trade names
Badamid®, Novamid®
Want to keep this datasheet? Save it now in your required format

Description

Partially aromatic copolyamide, 50% glass fiber reinforced, with high toughness and stability; injection moulding grade, heat aging stabilized

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.560 g/cm³

Show Material materials with Density of 1.560 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

16 GPa

Show Material materials with Elastic modulus of 16 GPa

Elongation

2.5 %

Show Material materials with Elongation of 2.5 %

Impact strength, Charpy notched

15 kJ/m²

Show Material materials with Impact strength, Charpy notched of 15 kJ/m²

Impact strength, Charpy unnotched

90 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 90 kJ/m²

Tensile strength

180 MPa

Show Material materials with Tensile strength of 180 MPa

at 2.5% strain

Thermal

PropertyValue

Melting point

295 °C

Show Material materials with Melting point of 295 °C

Flammability

UL 94 HB

Electrical

PropertyValue

Electrical resistivity

10000000000 Ω·m

Show Material materials with Electrical resistivity of 10000000000 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Fixing parts for kitchen devices

Fillers

50% Glass Fiber

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

Polymer Advanced Search

Processing methods

Injection molding