Polycarbonate + Poly(butylene terephthalate) (PC+PBT)

Alternative and trade names
Xenoy™, Edgetek™, Arnite®
Want to keep this datasheet? Save it now in your required format

Description

The key features are:


  • Long-term durability
  • High impact strength
  • Chemical resistance
  • Good surface appearance
  • Low shrinkage
  • Easy processing
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValue

    Density

    1.17 - 1.24 g/cm³

    Show Material materials with Density of 1.17 - 1.24 g/cm³

    Mechanical

    PropertyValueComment

    Elastic modulus

    1.8 - 2.5 GPa

    Show Material materials with Elastic modulus of 1.8 - 2.5 GPa

    Elongation

    80.0 - 150.0 %

    Show Material materials with Elongation of 80.0 - 150.0 %

    Impact strength, Charpy notched

    40.0 - 70.0 kJ/m²

    Show Material materials with Impact strength, Charpy notched of 40.0 - 70.0 kJ/m²

    Tensile strength

    40.0 - 65.0 MPa

    Show Material materials with Tensile strength of 40.0 - 65.0 MPa

    at 4-6% strain

    Impact strength, Charpy unnotched

    no break

    Thermal

    PropertyValue

    Coefficient of thermal expansion

    8e-05 - 0.00011 1/K

    Show Material materials with Coefficient of thermal expansion of 8e-05 - 0.00011 1/K

    Melting point

    220.0 - 225.0 °C

    Show Material materials with Melting point of 220.0 - 225.0 °C

    Thermal conductivity

    0.18 - 0.2 W/(m·K)

    Show Material materials with Thermal conductivity of 0.18 - 0.2 W/(m·K)

    Flammability

    UL 94 HB

    Electrical

    PropertyValue

    Dielectric constant

    3 [-]

    Show Material materials with Dielectric constant of 3 [-]

    3.5 [-]

    Show Material materials with Dielectric constant of 3.5 [-]

    Electrical resistivity

    10000000000000.0 - 1000000000000000.0 Ω·m

    Show Material materials with Electrical resistivity of 10000000000000.0 - 1000000000000000.0 Ω·m

    Optical

    PropertyValue

    Transparency

    no

    Technological properties

    Property
    Application areas

    Body panels, doorhandles, medical device enclosures, outdoor sport equipment

    Other

    You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

    Polymer Advanced Search

    Processing methods

    Injection molding