Reinforced polyamide with glass fiber. high temperature polyamide with halogen-free and halogen containing flame retardant grades for demanding applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries. That means a high temperature polyamide with a broad and versatile portfolio of grades that deliver high performance with a unique balance of properties.

Properties

General

Density ρ

1.43 - 1.47 g/cm³ at 20 °C

Mechanical

Elastic modulus E

10.5 - 12 GPa at 20 °C

Elongation A

1.5 - 2 % at 20 °C

Impact strength, Charpy notched Ivnot

5 - 10 kJ/m² at 20 °C

Impact strength, Charpy unnotched Iunnot

40 - 60 kJ/m² at 20 °C

Max allowed stress σmax

120 - 190 MPa at 20 °C

at 1.5-2% strain

Thermal

Coefficient of thermal expansion α

1.5E-5 - 7E-5 1/K at 20 °C

Flammability

UL 94 HB

Melting point Tm

325 °C

Electrical

Dielectric constant εr

3.9 - 5 [-] at 20 °C

Electrical resistivity ρel

1.00E+13 Ω·m at 20 °C

Optical

Transparency

no

Technological properties

Application areas

Crankshaft covers, automotive reflow connectors, e-motor bobbins, battery connectors

Fillers

30% Glass Fiber

Processing methods

Injection molding

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.