Polyamide 4T Reinforced with 30% Glass Fibers (PA4T+GF30)

Alternative and trade names
ForTii®
Want to keep this datasheet? Save it now in your required format

Description

Reinforced polyamide with glass fiber. high temperature polyamide with halogen-free and halogen containing flame retardant grades for demanding applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries. That means a high temperature polyamide with a broad and versatile portfolio of grades that deliver high performance with a unique balance of properties.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.43 - 1.47 g/cm³

Show Material materials with Density of 1.43 - 1.47 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

10.5 - 12.0 GPa

Show Material materials with Elastic modulus of 10.5 - 12.0 GPa

Elongation

1.5 - 2.0 %

Show Material materials with Elongation of 1.5 - 2.0 %

Impact strength, Charpy notched

5.0 - 10.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 5.0 - 10.0 kJ/m²

Impact strength, Charpy unnotched

40 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 40 kJ/m²

60 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 60 kJ/m²

Tensile strength

120.0 - 190.0 MPa

Show Material materials with Tensile strength of 120.0 - 190.0 MPa

at 1.5-2% strain

Thermal

PropertyValue

Coefficient of thermal expansion

1.5e-05 - 7e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.5e-05 - 7e-05 1/K

Melting point

325 °C

Show Material materials with Melting point of 325 °C

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

3.9 [-]

Show Material materials with Dielectric constant of 3.9 [-]

5 [-]

Show Material materials with Dielectric constant of 5 [-]

Electrical resistivity

10000000000000 Ω·m

Show Material materials with Electrical resistivity of 10000000000000 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Crankshaft covers, automotive reflow connectors, e-motor bobbins, battery connectors

Fillers

30% Glass Fiber

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: