SAE J775 Grade EV-14

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Reduction of area

20.0 °C

61 %

Show Material materials with Reduction of area of 61 %

650.0 °C

60 %

Show Material materials with Reduction of area of 60 %

760.0 °C

60 %

Show Material materials with Reduction of area of 60 %

Tensile strength

20.0 °C

880 MPa

Show Material materials with Tensile strength of 880 MPa

650.0 °C

490 MPa

Show Material materials with Tensile strength of 490 MPa

760.0 °C

320 MPa

Show Material materials with Tensile strength of 320 MPa

Unlock all property charts

Yield strength

20.0 °C

480 MPa

Show Material materials with Yield strength of 480 MPa

650.0 °C

220 MPa

Show Material materials with Yield strength of 220 MPa

760.0 °C

190 MPa

Show Material materials with Yield strength of 190 MPa

Unlock all property charts

Chemical properties

PropertyValue

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

Chromium

21 %

Show Material materials with Chromium of 21 %

Iron

66.2 - 100 %

Show Material materials with Iron of 66.2 - 100 %

Manganese

6.5 %

Show Material materials with Manganese of 6.5 %

Nickel

5.5 %

Show Material materials with Nickel of 5.5 %

Nitrogen

0.2 %

Show Material materials with Nitrogen of 0.2 %

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %