SAE J775 Grade EV-9

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.02 g/cm³

Show Material materials with Density of 8.02 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

195 GPa

Show Material materials with Elastic modulus of 195 GPa

Typical for Austenitic Stainless Steel

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Austenitic Stainless Steel

Reduction of area

20.0 °C

51 %

Show Material materials with Reduction of area of 51 %

650.0 °C

41 %

Show Material materials with Reduction of area of 41 %

760.0 °C

50 %

Show Material materials with Reduction of area of 50 %

Shear modulus

23.0 °C

77 GPa

Show Material materials with Shear modulus of 77 GPa

Typical for Austenitic Stainless Steel

Tensile strength

20.0 °C

880 MPa

Show Material materials with Tensile strength of 880 MPa

650.0 °C

52 MPa

Show Material materials with Tensile strength of 52 MPa

760.0 °C

320 MPa

Show Material materials with Tensile strength of 320 MPa

Unlock all property charts

Yield strength

20.0 °C

470 MPa

Show Material materials with Yield strength of 470 MPa

650.0 °C

230 MPa

Show Material materials with Yield strength of 230 MPa

760.0 °C

170 MPa

Show Material materials with Yield strength of 170 MPa

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

760.0 °C

1.93E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.93E-5 1/K

The mentioned value is between 20°C and the mentioned temperature

Melting point

1230 - 1480 °C

Show Material materials with Melting point of 1230 - 1480 °C

Typical for Austenitic Stainless Steel

Specific heat capacity

23.0 °C

440 J/(kg·K)

Show Material materials with Specific heat capacity of 440 J/(kg·K)

Typical for Austenitic Stainless Steel

Thermal conductivity

23.0 °C

11 - 21 W/(m·K)

Show Material materials with Thermal conductivity of 11 - 21 W/(m·K)

Typical for Austenitic Stainless Steel

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

8.5E-7 Ω·m

Show Material materials with Electrical resistivity of 8.5E-7 Ω·m

Typical for Austenitic Stainless Steel

Chemical properties

PropertyValueComment

Carbon

0.35 - 0.5 %

Show Material materials with Carbon of 0.35 - 0.5 %

Chromium

12 - 15 %

Show Material materials with Chromium of 12 - 15 %

Iron

64.2 - 73.65 %

Show Material materials with Iron of 64.2 - 73.65 %

Balance

Manganese

1 %

Show Material materials with Manganese of 1 %

Molybdenum

0.2 - 0.5 %

Show Material materials with Molybdenum of 0.2 - 0.5 %

Nickel

12 - 15 %

Show Material materials with Nickel of 12 - 15 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

0.3 - 0.8 %

Show Material materials with Silicon of 0.3 - 0.8 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Tungsten

1.5 - 3 %

Show Material materials with Tungsten of 1.5 - 3 %