General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Density of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 194 - 220 GPa Show Material materials with Elastic modulus of 194 - 220 GPa | Typical for Martensitic Stainless Steel |
Elongation A5 | 20.0 °C | 14 - 22 % Show Material materials with Elongation A5 of 14 - 22 % | |
Hardness, Brinell | 20.0 °C | 266 - 325 [-] Show Material materials with Hardness, Brinell of 266 - 325 [-] | |
Poisson's ratio | 20.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Martensitic Stainless Steel |
Reduction of area | 20.0 °C | 40 - 50 % Show Material materials with Reduction of area of 40 - 50 % | |
Tensile strength | 20.0 °C | 1100 - 1350 MPa Show Material materials with Tensile strength of 1100 - 1350 MPa | |
Yield strength | 20.0 °C | 750 MPa Show Material materials with Yield strength of 750 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.09E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.09E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
200.0 °C | 1.13E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.13E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
500.0 °C | 1.15E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.15E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
600.0 °C | 1.24E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.24E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
700.0 °C | 1.18E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.18E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.32E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.32E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1300.0 °C | 1.35E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.35E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Melting point | 1375 - 1450 °C Show Material materials with Melting point of 1375 - 1450 °C | Typical for Martensitic Stainless Steel | |
Specific heat capacity | 20.0 °C | 460 - 500 J/(kg·K) Show Material materials with Specific heat capacity of 460 - 500 J/(kg·K) | Typical for Martensitic Stainless Steel |
Thermal conductivity | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Thermal conductivity of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 20.0 °C | 6E-7 Ω·m Show Material materials with Electrical resistivity of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.4 - 0.5 % Show Material materials with Carbon of 0.4 - 0.5 % |
Chromium | 8 - 10 % Show Material materials with Chromium of 8 - 10 % |
Iron | Balance |
Manganese | 0.8 % Show Material materials with Manganese of 0.8 % |
Nickel | 0.6 % Show Material materials with Nickel of 0.6 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 2.7 - 3.3 % Show Material materials with Silicon of 2.7 - 3.3 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |