SAE J775 Grade XEV-E

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Reduction of area

20.0 °C

5 %

Show Material materials with Reduction of area of 5 %

760.0 °C

23 %

Show Material materials with Reduction of area of 23 %

Tensile strength

20.0 °C

770 MPa

Show Material materials with Tensile strength of 770 MPa

760.0 °C

520 MPa

Show Material materials with Tensile strength of 520 MPa

Unlock all property charts

Chemical properties

PropertyValue

Boron

1.5E-3 %

Show Material materials with Boron of 1.5E-3 %

Carbon

0.4 %

Show Material materials with Carbon of 0.4 %

Chromium

19 %

Show Material materials with Chromium of 19 %

Iron

66 - 100 %

Show Material materials with Iron of 66 - 100 %

Manganese

6.5 %

Show Material materials with Manganese of 6.5 %

Nickel

8 %

Show Material materials with Nickel of 8 %

Niobium

0.1 %

Show Material materials with Niobium of 0.1 %