SAE J775 Grade XEV-G

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.13 g/cm³

Show Material materials with Density of 8.13 g/cm³

Mechanical

PropertyTemperatureValue

Reduction of area

23.0 °C

16 %

Show Material materials with Reduction of area of 16 %

Tensile strength

23.0 °C

1120 MPa

Show Material materials with Tensile strength of 1120 MPa

Yield strength

23.0 °C

670 MPa

Show Material materials with Yield strength of 670 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

760.0 °C

1.53E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.53E-5 1/K

The mentioned value is between 20°C and the mentioned temperature

Chemical properties

PropertyValue

Aluminium

1 %

Show Material materials with Aluminium of 1 %

Carbon

0.1 %

Show Material materials with Carbon of 0.1 %

Chromium

27.8 %

Show Material materials with Chromium of 27.8 %

Iron

60.2 - 100 %

Show Material materials with Iron of 60.2 - 100 %

Manganese

8.5 %

Show Material materials with Manganese of 8.5 %

Nickel

0.4 %

Show Material materials with Nickel of 0.4 %