SAE J775 Grade XEV-I

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Reduction of area

23.0 °C

49 %

Show Material materials with Reduction of area of 49 %

Tensile strength

23.0 °C

1060 MPa

Show Material materials with Tensile strength of 1060 MPa

Yield strength

23.0 °C

970 MPa

Show Material materials with Yield strength of 970 MPa

Chemical properties

PropertyValue

Aluminium

0.5 %

Show Material materials with Aluminium of 0.5 %

Boron

0.05 %

Show Material materials with Boron of 0.05 %

Carbon

0.04 %

Show Material materials with Carbon of 0.04 %

Chromium

19 %

Show Material materials with Chromium of 19 %

Iron

21.21 - 100 %

Show Material materials with Iron of 21.21 - 100 %

Manganese

0.2 %

Show Material materials with Manganese of 0.2 %

Nickel

52.5 %

Show Material materials with Nickel of 52.5 %

Silicon

0.3 %

Show Material materials with Silicon of 0.3 %