General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation | 20.0 °C | 12 % Show Material materials with Elongation of 12 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 20.0 °C | 50 % Show Material materials with Reduction of area of 50 % | |
Tensile strength | 20.0 °C | 1000 - 1350 MPa Show Material materials with Tensile strength of 1000 - 1350 MPa | |
Yield strength | 20.0 °C | 800 - 900 MPa Show Material materials with Yield strength of 800 - 900 MPa |
Chemical properties
Property | Value |
---|---|
Boron | 8E-4 - 5E-3 % Show Material materials with Boron of 8E-4 - 5E-3 % |
Carbon | 0.36 - 0.42 % Show Material materials with Carbon of 0.36 - 0.42 % |
Chromium | 0.3 - 0.6 % Show Material materials with Chromium of 0.3 - 0.6 % |
Copper | 0.4 % Show Material materials with Copper of 0.4 % |
Manganese | 1.4 - 1.7 % Show Material materials with Manganese of 1.4 - 1.7 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.4 % Show Material materials with Silicon of 0.4 % |
Sulfur | 0.035 % Show Material materials with Sulfur of 0.035 % |