General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.85 g/cm³ Show Material materials with Density of 7.85 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 210 GPa Show Material materials with Elastic modulus of 210 GPa | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Shear modulus | 20.0 °C | 81 GPa Show Material materials with Shear modulus of 81 GPa | |
Tensile strength | 20.0 °C | 700 - 1000 MPa Show Material materials with Tensile strength of 700 - 1000 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.2E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K |
Specific heat capacity | 20.0 °C | 460 J/(kg·K) Show Material materials with Specific heat capacity of 460 J/(kg·K) |
Thermal conductivity | 20.0 °C | 44 W/(m·K) Show Material materials with Thermal conductivity of 44 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbon | 0.14 - 0.2 % Show Material materials with Carbon of 0.14 - 0.2 % |
Chromium | 0.6 - 0.9 % Show Material materials with Chromium of 0.6 - 0.9 % |
Copper | 0.4 % Show Material materials with Copper of 0.4 % |
Manganese | 0.4 - 0.7 % Show Material materials with Manganese of 0.4 - 0.7 % |
Nickel | 3 - 3.5 % Show Material materials with Nickel of 3 - 3.5 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.15 - 0.4 % Show Material materials with Silicon of 0.15 - 0.4 % |
Sulfur | 0.035 % Show Material materials with Sulfur of 0.035 % |