General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 200 GPa Show Material materials with Elastic modulus of 200 GPa | |
100.0 °C | 194 GPa Show Material materials with Elastic modulus of 194 GPa | ||
200.0 °C | 186 GPa Show Material materials with Elastic modulus of 186 GPa | ||
300.0 °C | 179 GPa Show Material materials with Elastic modulus of 179 GPa | ||
400.0 °C | 172 GPa Show Material materials with Elastic modulus of 172 GPa | ||
500.0 °C | 165 GPa Show Material materials with Elastic modulus of 165 GPa | ||
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Austenitic Stainless Steel |
Shear modulus | 23.0 °C | 77 GPa Show Material materials with Shear modulus of 77 GPa | Typical for Austenitic Stainless Steel |
Tensile strength | 20.0 °C | 1000 - 1150 MPa Show Material materials with Tensile strength of 1000 - 1150 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K | Typical for Austenitic Stainless Steel |
Melting point | 1230 - 1480 °C Show Material materials with Melting point of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Specific heat capacity | 23.0 °C | 440 J/(kg·K) Show Material materials with Specific heat capacity of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Thermal conductivity | 20.0 °C | 15 W/(m·K) Show Material materials with Thermal conductivity of 15 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | 7E-7 Ω·m Show Material materials with Electrical resistivity of 7E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Carbon | 0.15 % Show Material materials with Carbon of 0.15 % |
Chromium | 16 - 18 % Show Material materials with Chromium of 16 - 18 % |
Manganese | 5.5 - 7.5 % Show Material materials with Manganese of 5.5 - 7.5 % |
Nickel | 3.5 - 5.5 % Show Material materials with Nickel of 3.5 - 5.5 % |
Nitrogen | 0.05 - 0.25 % Show Material materials with Nitrogen of 0.05 - 0.25 % |
Phosphorus | 0.05 % Show Material materials with Phosphorus of 0.05 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |