Mechanical

PropertyTemperatureValue

Elongation A50

20.0 °C

18 %

Show Material materials with Elongation A50 of 18 %

Hardness, Brinell

20.0 °C

137 - 197 [-]

Show Material materials with Hardness, Brinell of 137 - 197 [-]

Reduction of area

20.0 °C

33 %

Show Material materials with Reduction of area of 33 %

Tensile strength

20.0 °C

485 - 655 MPa

Show Material materials with Tensile strength of 485 - 655 MPa

Yield Strength Rp0.2, short transverse

20.0 °C

250 MPa

Show Material materials with Yield Strength Rp0.2, short transverse of 250 MPa

Chemical properties

PropertyValue

Carbon

0.3 %

Show Material materials with Carbon of 0.3 %

Manganese

0.8 - 1.35 %

Show Material materials with Manganese of 0.8 - 1.35 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.15 - 0.35 %

Show Material materials with Silicon of 0.15 - 0.35 %

Sulfur

0.025 %

Show Material materials with Sulfur of 0.025 %