DIN 17745 Grade NiCo29-18 soft annealed (+A)

Want to keep this datasheet? Save it now in your required format

Description

Application: melting down in hard glass, glass/ceramic metal joints

Related Standards

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.2 g/cm³

Show Material materials with Density of 8.2 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

157 GPa

Show Material materials with Elastic modulus of 157 GPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

100.0 °C

6.5E-6 1/K

Show Material materials with Coefficient of thermal expansion of 6.5E-6 1/K

150.0 °C

6.2E-6 1/K

Show Material materials with Coefficient of thermal expansion of 6.2E-6 1/K

200.0 °C

5.9E-6 1/K

Show Material materials with Coefficient of thermal expansion of 5.9E-6 1/K

300.0 °C

5.4E-6 1/K

Show Material materials with Coefficient of thermal expansion of 5.4E-6 1/K

400.0 °C

5.1E-6 1/K

Show Material materials with Coefficient of thermal expansion of 5.1E-6 1/K

500.0 °C

6.2E-6 1/K

Show Material materials with Coefficient of thermal expansion of 6.2E-6 1/K

600.0 °C

7.8E-6 1/K

Show Material materials with Coefficient of thermal expansion of 7.8E-6 1/K

Thermal conductivity

20.0 °C

17 W/(m·K)

Show Material materials with Thermal conductivity of 17 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

4.5E-7 Ω·m

Show Material materials with Electrical resistivity of 4.5E-7 Ω·m

Chemical properties

PropertyValue

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Cobalt

16 - 18 %

Show Material materials with Cobalt of 16 - 18 %

Manganese

0.5 %

Show Material materials with Manganese of 0.5 %

Nickel

28 - 30 %

Show Material materials with Nickel of 28 - 30 %

Silicon

0.3 %

Show Material materials with Silicon of 0.3 %