JIS G4307 Grade SUS304N1

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.9 - 8.2 g/cm³

Show Material materials with Density of 7.9 - 8.2 g/cm³

Typical for Austenitic Stainless Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

195 GPa

Show Material materials with Elastic modulus of 195 GPa

Typical for Austenitic Stainless Steel

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Austenitic Stainless Steel

Shear modulus

23.0 °C

77 GPa

Show Material materials with Shear modulus of 77 GPa

Typical for Austenitic Stainless Steel

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.7E-5 - 1.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K

Typical for Austenitic Stainless Steel

Melting point

1230 - 1480 °C

Show Material materials with Melting point of 1230 - 1480 °C

Typical for Austenitic Stainless Steel

Specific heat capacity

23.0 °C

440 J/(kg·K)

Show Material materials with Specific heat capacity of 440 J/(kg·K)

Typical for Austenitic Stainless Steel

Thermal conductivity

23.0 °C

11 - 21 W/(m·K)

Show Material materials with Thermal conductivity of 11 - 21 W/(m·K)

Typical for Austenitic Stainless Steel

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

8.5E-7 Ω·m

Show Material materials with Electrical resistivity of 8.5E-7 Ω·m

Typical for Austenitic Stainless Steel

Chemical properties

PropertyValue

Carbon

0.08 %

Show Material materials with Carbon of 0.08 %

Chromium

18 - 20 %

Show Material materials with Chromium of 18 - 20 %

Iron

65.59 - 74.9 %

Show Material materials with Iron of 65.59 - 74.9 %

Manganese

2.5 %

Show Material materials with Manganese of 2.5 %

Nickel

7 - 10.5 %

Show Material materials with Nickel of 7 - 10.5 %

Nitrogen

0.1 - 0.25 %

Show Material materials with Nitrogen of 0.1 - 0.25 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %