General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.12 - 0.18 % Show Material materials with Carbon of 0.12 - 0.18 % |
Chromium | 0.2 - 0.5 % Show Material materials with Chromium of 0.2 - 0.5 % |
Iron | 95.76 - 97.18 % Show Material materials with Iron of 95.76 - 97.18 % |
Manganese | 0.35 - 0.65 % Show Material materials with Manganese of 0.35 - 0.65 % |
Nickel | 2 - 2.5 % Show Material materials with Nickel of 2 - 2.5 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.15 - 0.35 % Show Material materials with Silicon of 0.15 - 0.35 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |