JIS G4105 Grade SCM435

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperatureComment

Density

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³ at 23.0 °C

23.0 °C

Typical for Chromium Molybdenum Steel

Mechanical

PropertyValueTemperatureComment

Elastic modulus

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa at 23.0 °C

23.0 °C

Typical for Chromium Molybdenum Steel

Poisson's ratio

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-] at 23.0 °C

23.0 °C

Typical for Chromium Molybdenum Steel

Thermal

PropertyValueTemperatureComment

Coefficient of thermal expansion

1.1E-5 - 1.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K at 23.0 °C

23.0 °C

Typical for Chromium Molybdenum Steel

Melting point

1382 - 1529 °C

Show Material materials with Melting point of 1382 - 1529 °C

Typical for Chromium Molybdenum Steel

Specific heat capacity

448 - 502 J/(kg·K)

Show Material materials with Specific heat capacity of 448 - 502 J/(kg·K) at 23.0 °C

23.0 °C

Typical for Chromium Molybdenum Steel

Thermal conductivity

36 - 43 W/(m·K)

Show Material materials with Thermal conductivity of 36 - 43 W/(m·K) at 23.0 °C

23.0 °C

Typical for Chromium Molybdenum Steel

Chemical properties

Property

Carbon

0.33 - 0.38 %

Chromium

0.9 - 1.2 %

Iron

96.86 - 97.87 %

Manganese

0.6 - 0.85 %

Molybdenum

0.15 - 0.3 %

Phosphorus

0.03 %

Silicon

0.15 - 0.35 %

Sulfur

0.03 %