General
Property | Value | Comment |
---|---|---|
Density | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Low Carbon Steel |
Poisson's ratio | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Low Carbon Steel |
Shear modulus | 82 GPa Show Material materials with Shear modulus of 82 GPa | Typical for Low Carbon Steel |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Max service temperature | 500 °C Show Material materials with Max service temperature of 500 °C | Typical for Carbon Steel |
Melting point | 1480 - 1526 °C Show Material materials with Melting point of 1480 - 1526 °C | Typical for Low Carbon Steel |
Specific heat capacity | 465 J/(kg·K) Show Material materials with Specific heat capacity of 465 J/(kg·K) | Typical for Low Carbon Steel |
Thermal conductivity | 25 - 93 W/(m·K) Show Material materials with Thermal conductivity of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Electrical
Property | Value | Comment |
---|---|---|
Electrical resistivity | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Electrical resistivity of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnetic
Property | Value | Comment |
---|---|---|
Curie temperature | 770 °C Show Material materials with Curie temperature of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Carbon | 0.08 % Show Material materials with Carbon of 0.08 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Chromium | 0.02 % Show Material materials with Chromium of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Copper | 0.02 % Show Material materials with Copper of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Manganese | 0.45 % Show Material materials with Manganese of 0.45 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Molybdenum | 0.02 % Show Material materials with Molybdenum of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Nickel | 0.02 % Show Material materials with Nickel of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Niobium | 0.08 % Show Material materials with Niobium of 0.08 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Silicon | 0.02 % Show Material materials with Silicon of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Sulfur | 0.035 % Show Material materials with Sulfur of 0.035 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Titanium | 0.08 % Show Material materials with Titanium of 0.08 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Vanadium | 0.08 % Show Material materials with Vanadium of 0.08 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |