General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Manganese Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Manganese Steel |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Manganese Steel |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.33E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.33E-5 1/K | Typical for Manganese Steel |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Manganese Steel | |
Specific heat capacity | 23.0 °C | 510 - 553 J/(kg·K) Show Material materials with Specific heat capacity of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
Thermal conductivity | 23.0 °C | 14 - 16 W/(m·K) Show Material materials with Thermal conductivity of 14 - 16 W/(m·K) | Typical for Manganese Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Carbon | 0.4 - 0.48 % Show Material materials with Carbon of 0.4 - 0.48 % |
Chromium | 0.02 % Show Material materials with Chromium of 0.02 % |
Copper | 0.02 % Show Material materials with Copper of 0.02 % |
Iron | balance |
Manganese | 1.35 - 1.65 % Show Material materials with Manganese of 1.35 - 1.65 % |
Molybdenum | 0.02 % Show Material materials with Molybdenum of 0.02 % |
Nickel | 0.02 % Show Material materials with Nickel of 0.02 % |
Niobium | 0.08 % Show Material materials with Niobium of 0.08 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.02 % Show Material materials with Silicon of 0.02 % |
Sulfur | 0.24 - 0.33 % Show Material materials with Sulfur of 0.24 - 0.33 % |
Titanium | 0.08 % Show Material materials with Titanium of 0.08 % |
Vanadium | 0.08 % Show Material materials with Vanadium of 0.08 % |