General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 206 GPa Show Material materials with Elastic modulus of 206 GPa | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 20.0 °C | 30 - 40 % Show Material materials with Reduction of area of 30 - 40 % | |
Shear modulus | 20.0 °C | 81.5 GPa Show Material materials with Shear modulus of 81.5 GPa | |
Tensile strength | 20.0 °C | 1160 - 2200 MPa Show Material materials with Tensile strength of 1160 - 2200 MPa |
Thermal
Property | Value |
---|---|
Max service temperature, long | -15 - 80 °C Show Material materials with Max service temperature, long of -15 - 80 °C |
Chemical properties
Property | Value |
---|---|
Carbon | 0.7 - 1 % Show Material materials with Carbon of 0.7 - 1 % |
Copper | 0.12 % Show Material materials with Copper of 0.12 % |
Manganese | 0.3 - 1.5 % Show Material materials with Manganese of 0.3 - 1.5 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.35 % Show Material materials with Silicon of 0.35 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |
Technological properties
Property | ||
---|---|---|
Features | Spring |