General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.86 g/cm³ Show Material materials with Density of 7.86 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 207 GPa Show Material materials with Elastic modulus of 207 GPa |
100.0 °C | 203 GPa Show Material materials with Elastic modulus of 203 GPa | |
200.0 °C | 197 GPa Show Material materials with Elastic modulus of 197 GPa | |
300.0 °C | 189 GPa Show Material materials with Elastic modulus of 189 GPa | |
400.0 °C | 181 GPa Show Material materials with Elastic modulus of 181 GPa | |
500.0 °C | 172 GPa Show Material materials with Elastic modulus of 172 GPa | |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.15E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.15E-5 1/K |
200.0 °C | 1.2E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K | |
300.0 °C | 1.24E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.24E-5 1/K | |
400.0 °C | 1.28E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.28E-5 1/K | |
500.0 °C | 1.31E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.31E-5 1/K | |
600.0 °C | 1.35E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.35E-5 1/K | |
Specific heat capacity | 20.0 °C | 464 J/(kg·K) Show Material materials with Specific heat capacity of 464 J/(kg·K) |
100.0 °C | 479 J/(kg·K) Show Material materials with Specific heat capacity of 479 J/(kg·K) | |
200.0 °C | 496 J/(kg·K) Show Material materials with Specific heat capacity of 496 J/(kg·K) | |
300.0 °C | 513 J/(kg·K) Show Material materials with Specific heat capacity of 513 J/(kg·K) | |
400.0 °C | 532 J/(kg·K) Show Material materials with Specific heat capacity of 532 J/(kg·K) | |
Thermal conductivity | 20.0 °C | 32.9 W/(m·K) Show Material materials with Thermal conductivity of 32.9 W/(m·K) |
100.0 °C | 34.2 W/(m·K) Show Material materials with Thermal conductivity of 34.2 W/(m·K) | |
200.0 °C | 34.8 W/(m·K) Show Material materials with Thermal conductivity of 34.8 W/(m·K) | |
300.0 °C | 34.4 W/(m·K) Show Material materials with Thermal conductivity of 34.4 W/(m·K) | |
400.0 °C | 33.3 W/(m·K) Show Material materials with Thermal conductivity of 33.3 W/(m·K) | |
Thermal diffusivity | 20.0 °C | 9 mm²/s Show Material materials with Thermal diffusivity of 9 mm²/s |
100.0 °C | 8.8 mm²/s Show Material materials with Thermal diffusivity of 8.8 mm²/s | |
200.0 °C | 8.5 mm²/s Show Material materials with Thermal diffusivity of 8.5 mm²/s | |
300.0 °C | 7.8 mm²/s Show Material materials with Thermal diffusivity of 7.8 mm²/s | |
400.0 °C | 7.1 mm²/s Show Material materials with Thermal diffusivity of 7.1 mm²/s | |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | 3.17E-7 Ω·m Show Material materials with Electrical resistivity of 3.17E-7 Ω·m |
100.0 °C | 3.74E-7 Ω·m Show Material materials with Electrical resistivity of 3.74E-7 Ω·m | |
200.0 °C | 4.54E-7 Ω·m Show Material materials with Electrical resistivity of 4.54E-7 Ω·m | |
300.0 °C | 5.46E-7 Ω·m Show Material materials with Electrical resistivity of 5.46E-7 Ω·m | |
400.0 °C | 6.53E-7 Ω·m Show Material materials with Electrical resistivity of 6.53E-7 Ω·m | |
Chemical properties
Property | Value |
---|---|
Carbon | 0.16 - 0.22 % Show Material materials with Carbon of 0.16 - 0.22 % |
Chromium | 1.1 - 1.4 % Show Material materials with Chromium of 1.1 - 1.4 % |
Manganese | 0.15 - 0.45 % Show Material materials with Manganese of 0.15 - 0.45 % |
Molybdenum | 0.15 - 0.25 % Show Material materials with Molybdenum of 0.15 - 0.25 % |
Nickel | 3.8 - 4.3 % Show Material materials with Nickel of 3.8 - 4.3 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.1 - 0.4 % Show Material materials with Silicon of 0.1 - 0.4 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |
Tungsten | 0.3 - 0.5 % Show Material materials with Tungsten of 0.3 - 0.5 % |