DIN 17465 Grade G-CoCr28 cast condition

Want to keep this datasheet? Save it now in your required format

Description

According to DIN EN 10295 : 2003-01, the highest temperature in air is 1200 °C for the material G-CoCr28, material number 2.4778 . For cyclic heatings, the highest temperature in air is 1100 °C. The following is valid for the comparable austenitic DIN-material: The heat-resistant cast material G-CoCr28 is also produced as the wrought material CoCr28 (material number 2.4778 as well). It is applied in the construction of industrial furnaces at up to 1100 °C. Its weldability is good, a preheating is not necessary.

Related Standards

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.1 g/cm³

Show Material materials with Density of 8.1 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Elongation

20.0 °C

6 %

Show Material materials with Elongation of 6 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

20.0 °C

490 MPa

Show Material materials with Tensile strength of 490 MPa

Yield strength Rp0.2

20.0 °C

235 MPa

Show Material materials with Yield strength Rp0.2 of 235 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

400.0 °C

1.5E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.5E-5 1/K

800.0 °C

1.6E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.6E-5 1/K

1000.0 °C

1.7E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K

Max service temperature, long

0 - 1200 °C

Show Material materials with Max service temperature, long of 0 - 1200 °C

Specific heat capacity

20.0 °C

500 J/(kg·K)

Show Material materials with Specific heat capacity of 500 J/(kg·K)

Thermal conductivity

20.0 °C

8.5 - 9.2 W/(m·K)

Show Material materials with Thermal conductivity of 8.5 - 9.2 W/(m·K)

800.0 °C

21 W/(m·K)

Show Material materials with Thermal conductivity of 21 W/(m·K)

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

8.25E-7 Ω·m

Show Material materials with Electrical resistivity of 8.25E-7 Ω·m

Chemical properties

PropertyValue

Carbon

0.05 - 0.25 %

Show Material materials with Carbon of 0.05 - 0.25 %

Chromium

27 - 30 %

Show Material materials with Chromium of 27 - 30 %

Cobalt

48 - 52 %

Show Material materials with Cobalt of 48 - 52 %

Iron

9.68 %

Show Material materials with Iron of 9.68 %

Manganese

1.5 %

Show Material materials with Manganese of 1.5 %

Molybdenum

0.5 %

Show Material materials with Molybdenum of 0.5 %

Nickel

4 %

Show Material materials with Nickel of 4 %

Niobium

0.5 %

Show Material materials with Niobium of 0.5 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.5 - 1.5 %

Show Material materials with Silicon of 0.5 - 1.5 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %