DIN 41301 Grade D1a fully processed

Want to keep this datasheet? Save it now in your required format

Description

Steel with specific requirements for the permeability at low field strengths. Application: audio-frequency transformers in communications technology (sheets, strips, core laminations, tape cores)

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.15 g/cm³

Show Material materials with Density of 8.15 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for Nickel Steel

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Nickel Steel

Shear modulus

23.0 °C

76 GPa

Show Material materials with Shear modulus of 76 GPa

Typical for Nickel Steel

Thermal

PropertyTemperatureValueComment

Melting point

1316 - 1595 °C

Show Material materials with Melting point of 1316 - 1595 °C

Typical for Nickel Steel

Specific heat capacity

23.0 °C

456 J/(kg·K)

Show Material materials with Specific heat capacity of 456 J/(kg·K)

Typical for Nickel Steel

Thermal conductivity

23.0 °C

10 - 50 W/(m·K)

Show Material materials with Thermal conductivity of 10 - 50 W/(m·K)

Typical for Nickel Steel

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

7.5E-7 Ω·m

Show Material materials with Electrical resistivity of 7.5E-7 Ω·m

Chemical properties

PropertyValue

Nickel

36 - 40 %

Show Material materials with Nickel of 36 - 40 %