Ni-Fe alloy with specific requirements for the permeability at low field strengths. Application: audio-frequency transformers in communications technology (sheets, strips, core laminations, tape cores) Source material acc. to DIN 17745: 2.4505, 2.4525, 2.4545 und 2.4405

Related Standards

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.7 g/cm³

Show Material materials with Density of 8.7 g/cm³

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

5.5E-7 Ω·m

Show Material materials with Electrical resistivity of 5.5E-7 Ω·m

Chemical properties

PropertyValue

Nickel

75 %

Show Material materials with Nickel of 75 %