DIN 43720 Grade X10NiCr32-20 quenched (+Q)

Want to keep this datasheet? Save it now in your required format

Description

Heat resistance in air: up to 1200 °C. Application: tubes in the petroleum industry

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.9 g/cm³

Show Material materials with Density of 7.9 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Elongation

20.0 °C

30 %

Show Material materials with Elongation of 30 %

Hardness, Brinell

20.0 °C

200 [-]

Show Material materials with Hardness, Brinell of 200 [-]

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

20.0 °C

490 - 740 MPa

Show Material materials with Tensile strength of 490 - 740 MPa

Yield strength Rp0.2

20.0 °C

235 MPa

Show Material materials with Yield strength Rp0.2 of 235 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

400.0 °C

1.6E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.6E-5 1/K

800.0 °C

1.75E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.75E-5 1/K

1000.0 °C

1.85E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.85E-5 1/K

Specific heat capacity

20.0 °C

500 J/(kg·K)

Show Material materials with Specific heat capacity of 500 J/(kg·K)

Thermal conductivity

20.0 °C

12 W/(m·K)

Show Material materials with Thermal conductivity of 12 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

1.04E-6 Ω·m

Show Material materials with Electrical resistivity of 1.04E-6 Ω·m

Chemical properties

PropertyValue

Carbon

0.12 %

Show Material materials with Carbon of 0.12 %

Chromium

19 - 22 %

Show Material materials with Chromium of 19 - 22 %

Manganese

1.5 %

Show Material materials with Manganese of 1.5 %

Nickel

30 - 34 %

Show Material materials with Nickel of 30 - 34 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %