General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 7.85 g/cm³ Show Material materials with Density of 7.85 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | In Normalized Condition |
Elongation | 23.0 °C | 7 - 18 % Show Material materials with Elongation of 7 - 18 % | For Different Conditions |
Hardness, Brinell | 23.0 °C | 197 [-] Show Material materials with Hardness, Brinell of 197 [-] | |
Hardness, Rockwell B | 23.0 °C | 92 [-] Show Material materials with Hardness, Rockwell B of 92 [-] | |
Poisson's ratio | 23.0 °C | 0.27 [-] Show Material materials with Poisson's ratio of 0.27 [-] | In Normalized Condition |
Shear modulus | 23.0 °C | 75 - 80 GPa Show Material materials with Shear modulus of 75 - 80 GPa | Typical for Carbon Steel |
Tensile strength | 23.0 °C | 630 - 950 MPa Show Material materials with Tensile strength of 630 - 950 MPa | For Different Conditions |
Yield strength | 23.0 °C | 560 MPa Show Material materials with Yield strength of 560 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.32E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.32E-5 1/K | Typical for Medium Carbon Steel |
Max service temperature | 500 °C Show Material materials with Max service temperature of 500 °C | Typical for Carbon Steel | |
Melting point | 1380 - 1514 °C Show Material materials with Melting point of 1380 - 1514 °C | Typical for Medium Carbon Steel | |
Specific heat capacity | 23.0 °C | 470 - 520 J/(kg·K) Show Material materials with Specific heat capacity of 470 - 520 J/(kg·K) | Typical for Medium Carbon Steel |
Thermal conductivity | 23.0 °C | 21 - 52 W/(m·K) Show Material materials with Thermal conductivity of 21 - 52 W/(m·K) | Typical for Medium Carbon Steel |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.5 - 0.6 % Show Material materials with Carbon of 0.5 - 0.6 % |
Manganese | 0.6 - 0.9 % Show Material materials with Manganese of 0.6 - 0.9 % |
Technological properties
Property | ||
---|---|---|
Corrosion properties | Not Corrosion Resistance |