Mechanical

PropertyTemperatureValueComment

Charpy impact energy, V-notch

-12 °C

27

Show Material materials with Charpy impact energy, V-notch of 27

average

4 °C

27

Show Material materials with Charpy impact energy, V-notch of 27

average

21 °C

27

Show Material materials with Charpy impact energy, V-notch of 27

average

Elongation

18.0 - 21.0 %

Show Material materials with Elongation of 18.0 - 21.0 %

Tensile strength

485 MPa

Show Material materials with Tensile strength of 485 MPa

min.

Chemical properties

PropertyValueComment

Aluminium

0.01 - 0.04 %

Show Material materials with Aluminium of 0.01 - 0.04 %

Carbon

0.11

Show Material materials with Carbon of 0.11

max.

Chromium

0.45 - 0.7000000000000001 %

Show Material materials with Chromium of 0.45 - 0.7000000000000001 %

Copper

0.25 - 0.4 %

Show Material materials with Copper of 0.25 - 0.4 %

Manganese

1.1 - 1.5 %

Show Material materials with Manganese of 1.1 - 1.5 %

Molybdenum

0.02 - 0.08 %

Show Material materials with Molybdenum of 0.02 - 0.08 %

Nickel

0.25 - 0.4 %

Show Material materials with Nickel of 0.25 - 0.4 %

Nitrogen

0.015

Show Material materials with Nitrogen of 0.015

max.

Phosphorus

0.2

Show Material materials with Phosphorus of 0.2

max.

Silicon

0.30000000000000004 - 0.5 %

Show Material materials with Silicon of 0.30000000000000004 - 0.5 %

Sulfur

0.006

Show Material materials with Sulfur of 0.006

max.

Vanadium

0.04 - 0.08 %