ABS Grade FQ43

Want to keep this datasheet? Save it now in your required format

Description

Extra High Strength Steel

Related Standards

This material data has been provided by ABS Standard.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Carbon equivalent (CEV)

0.43 [-]

Show Material materials with Carbon equivalent (CEV) of 0.43 [-]

for t ≤ 50 mm plate thickness condition TM

0.44 [-]

Show Material materials with Carbon equivalent (CEV) of 0.44 [-]

for t ≤ 50 mm sections condition TM

0.45 [-]

Show Material materials with Carbon equivalent (CEV) of 0.45 [-]

for 50 < t ≤100 mm plate thickness condition TM

0.45 [-]

Show Material materials with Carbon equivalent (CEV) of 0.45 [-]

for t ≤ 50 mm plate thickness condition QT

0.46 [-]

Show Material materials with Carbon equivalent (CEV) of 0.46 [-]

for t ≤ 50 mm plate thickness condition N/NR

0.47 [-]

Show Material materials with Carbon equivalent (CEV) of 0.47 [-]

for t ≤ 50 mm sections condition N/NR

0.47 [-]

Show Material materials with Carbon equivalent (CEV) of 0.47 [-]

for t ≤ 65 mm tabulars condition N/NR

0.47 [-]

Show Material materials with Carbon equivalent (CEV) of 0.47 [-]

for 100 < t ≤ 250 mm plate thickness condition TM

0.47 [-]

Show Material materials with Carbon equivalent (CEV) of 0.47 [-]

for 50 < t ≤100 mm plate thickness condition QT

0.48 [-]

Show Material materials with Carbon equivalent (CEV) of 0.48 [-]

for 50 < t ≤100 mm plate thickness condition N/NR

0.49 [-]

Show Material materials with Carbon equivalent (CEV) of 0.49 [-]

for 100 < t ≤ 250 mm plate thickness condition QT

0.52 [-]

Show Material materials with Carbon equivalent (CEV) of 0.52 [-]

for 100 < t ≤ 250 mm plate thickness condition N/NR

0.53 [-]

Show Material materials with Carbon equivalent (CEV) of 0.53 [-]

for t ≤ 250 or d ≤ 250 mm bars condition N/NR

Density

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

typical for low carbon steel

Mechanical

PropertyTemperatureValueComment

Charpy impact energy, V-notch

-60.0 °C

41.0 J

Show Material materials with Charpy impact energy, V-notch of 41.0 J

Charpy impact energy, V-notch, transverse

-60.0 °C

27.0 J

Show Material materials with Charpy impact energy, V-notch, transverse of 27.0 J

Elastic modulus

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

typical for low carbon steel

Elongation

18 %

Show Material materials with Elongation of 18 %

min.

Poisson's ratio

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

typical for low carbon steel

Shear modulus

82 GPa

Show Material materials with Shear modulus of 82 GPa

typical for low carbon steel

Tensile strength

530 - 680 MPa

Show Material materials with Tensile strength of 530 - 680 MPa

Thermal

PropertyValueComment

Coefficient of thermal expansion

1.32e-05 - 1.38e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.32e-05 - 1.38e-05 1/K

typical for low carbon steel

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

typical for carbon steel

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

typical for low carbon steel

Specific heat capacity

465 J/(kg·K)

Show Material materials with Specific heat capacity of 465 J/(kg·K)

typical for low carbon steel

Thermal conductivity

25 - 93 W/(m·K)

Show Material materials with Thermal conductivity of 25 - 93 W/(m·K)

typical for low carbon steel

Electrical

PropertyValueComment

Electrical resistivity

1.43e-07 - 1.74e-07 Ω·m

Show Material materials with Electrical resistivity of 1.43e-07 - 1.74e-07 Ω·m

typical for carbon steel

Chemical properties

PropertyValueComment

Aluminium

0.018 - 0.2 %

Show Material materials with Aluminium of 0.018 - 0.2 %

min., depending on the delivery condition

Boron

0.005 %

Show Material materials with Boron of 0.005 %

max.

Calcium

0.005 %

Show Material materials with Calcium of 0.005 %

max.

Carbon

0.14 - 0.18 %

Show Material materials with Carbon of 0.14 - 0.18 %

max., depending on the delivery condition

Chromium

0.3 - 2 %

Show Material materials with Chromium of 0.3 - 2 %

max., depending on the delivery condition

Copper

0.5 - 0.55 %

Show Material materials with Copper of 0.5 - 0.55 %

max., depending on the delivery condition

Manganese

1 - 1.7 %

Show Material materials with Manganese of 1 - 1.7 %

depending on the delivery condition

Molybdenum

0.1 - 0.7 %

Show Material materials with Molybdenum of 0.1 - 0.7 %

max., depending on the delivery condition

Nickel

0.8 - 3.5 %

Show Material materials with Nickel of 0.8 - 3.5 %

max., depending on the delivery condition

Niobium

0.05 - 0.06 %

Show Material materials with Niobium of 0.05 - 0.06 %

max., depending on the delivery condition

Nitrogen

0.015 - 0.025 %

Show Material materials with Nitrogen of 0.015 - 0.025 %

max., depending on the delivery condition

Oxygen

0.003 - 0.005 %

Show Material materials with Oxygen of 0.003 - 0.005 %

max., depending on the delivery condition

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

max., depending on the delivery condition

Silicon

0.6 - 0.8 %

Show Material materials with Silicon of 0.6 - 0.8 %

max., depending on the delivery condition

Sulfur

0.01 %

Show Material materials with Sulfur of 0.01 %

max., depending on the delivery condition

Titanium

0.05 %

Show Material materials with Titanium of 0.05 %

max.

Vanadium

0.12 - 0.2 %

Show Material materials with Vanadium of 0.12 - 0.2 %

max., depending on the delivery condition

Technological properties

Property
Supplier Disclaimer

The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information.