Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 20.0 °C | 15 - 17 % Show Material materials with Elongation of 15 - 17 % |
Hardness, Brinell | 20.0 °C | 201 - 255 [-] Show Material materials with Hardness, Brinell of 201 - 255 [-] |
Tensile strength | 20.0 °C | 700 - 850 MPa Show Material materials with Tensile strength of 700 - 850 MPa |
Yield strength | 20.0 °C | 495 - 525 MPa Show Material materials with Yield strength of 495 - 525 MPa |
Yield strength Rp0.2 | 20.0 °C | 480 - 510 MPa Show Material materials with Yield strength Rp0.2 of 480 - 510 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.32 - 0.4 % Show Material materials with Carbon of 0.32 - 0.4 % |
Iron | Balance |
Manganese | 1.3 - 1.7 % Show Material materials with Manganese of 1.3 - 1.7 % |
Molybdenum | 0.22 - 0.32 % Show Material materials with Molybdenum of 0.22 - 0.32 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 0.1 - 0.4 % Show Material materials with Silicon of 0.1 - 0.4 % |
Sulfur | 0.04 % Show Material materials with Sulfur of 0.04 % |