General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Medium Carbon Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Medium Carbon Steel |
Elongation | 20.0 °C | 10 % Show Material materials with Elongation of 10 % | |
Hardness, HBW | 20.0 °C | 207 - 225 [-] Show Material materials with Hardness, HBW of 207 - 225 [-] | |
Poisson's ratio | 20.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Medium Carbon Steel |
Shear modulus | 20.0 °C | 75 - 80 GPa Show Material materials with Shear modulus of 75 - 80 GPa | Typical for Carbon Steel |
Tensile strength | 20.0 °C | 690 MPa Show Material materials with Tensile strength of 690 MPa | |
Yield strength | 20.0 °C | 485 MPa Show Material materials with Yield strength of 485 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1.32E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.32E-5 1/K | Typical for Medium Carbon Steel |
Max service temperature | 500 °C Show Material materials with Max service temperature of 500 °C | Typical for Carbon Steel | |
Melting point | 1380 - 1514 °C Show Material materials with Melting point of 1380 - 1514 °C | Typical for Medium Carbon Steel |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 20.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Carbon | 0.4 - 0.5 % Show Material materials with Carbon of 0.4 - 0.5 % | |
Iron | 97.69 - 99.1 % Show Material materials with Iron of 97.69 - 99.1 % | balance |
Manganese | 0.5 - 0.9 % Show Material materials with Manganese of 0.5 - 0.9 % | |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % | |
Silicon | 0.8 % Show Material materials with Silicon of 0.8 % | |
Sulfur | 0.045 % Show Material materials with Sulfur of 0.045 % |