EN 10139 Grade USt 3 cold rolled, skin passed (K32)

Want to keep this datasheet? Save it now in your required format

Description

The soft non-alloy steel USt 3 is suited for cold forming and is offered in different conditions (K to K60) with different strength and depth indications. The steel is applicated in the plant and tool engineering. Free from stretcher lines for 4 weeks is garuanteed in the LG and K32 condition. No stretcher lines occur in the conditions K40 to K60. The steel is weldable, in the conditions K32 to K40 the strength can be decreased post welding.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for Low Carbon Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for Low Carbon Steel

Elongation

20.0 °C

26 %

Show Material materials with Elongation of 26 %

Elongation A80

20.0 °C

22 %

Show Material materials with Elongation A80 of 22 %

Poisson's ratio

20.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Low Carbon Steel

Tensile strength

20.0 °C

290 - 390 MPa

Show Material materials with Tensile strength of 290 - 390 MPa

Yield strength

20.0 °C

210 - 355 MPa

Show Material materials with Yield strength of 210 - 355 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

1.32E-5 - 1.38E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K

Typical for Low Carbon Steel

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

Typical for Low Carbon Steel

Magnetic

PropertyValueComment

Curie temperature

770 °C

Show Material materials with Curie temperature of 770 °C

Typical for Low Carbon Steel

Chemical properties

PropertyValue

Carbon

0.08 %

Show Material materials with Carbon of 0.08 %

Nitrogen

7E-3 %

Show Material materials with Nitrogen of 7E-3 %

Do you have a technical question or need more information about this material?

Post it as a comment below and receive answers from engineers and other community members.