DIN 1654-5 Grade X10Cr13 annealed to achieve spheroidized carbides, cold worked (+AC+C)

View suppliers (2)
Want to keep this datasheet? Save it now in your required format

Description

The steel X10Cr13 is well suited for cold-forming in the annealed condition. The strain hardening inclination is significantly lower than that of stainless austenitic steels and is about equal to that of a carbon steel. It is used for construction parts operating in water and steam, and for mild media in the food industry, predominantly in the tempered condition (screws and molded parts). Temperature of use: up to 550 degrees C.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.73 g/cm³

Show Material materials with Density of 7.73 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

217 - 217.99 GPa

Show Material materials with Elastic modulus of 217 - 217.99 GPa

100.0 °C

213.2 - 215 GPa

Show Material materials with Elastic modulus of 213.2 - 215 GPa

200.0 °C

188 - 205.94 GPa

Show Material materials with Elastic modulus of 188 - 205.94 GPa

300.0 °C

164 - 198.53 GPa

Show Material materials with Elastic modulus of 164 - 198.53 GPa

400.0 °C

188.79 GPa

Show Material materials with Elastic modulus of 188.79 GPa

Poisson's ratio

20.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

100.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

200.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

300.0 °C

0.31 [-]

Show Material materials with Poisson's ratio of 0.31 [-]

400.0 °C

0.31 [-]

Show Material materials with Poisson's ratio of 0.31 [-]

Unlock all property charts

Reduction of area

20.0 °C

60 %

Show Material materials with Reduction of area of 60 %

Shear modulus

20.0 °C

84.82 GPa

Show Material materials with Shear modulus of 84.82 GPa

100.0 °C

82.5 GPa

Show Material materials with Shear modulus of 82.5 GPa

200.0 °C

79.57 GPa

Show Material materials with Shear modulus of 79.57 GPa

300.0 °C

75.86 GPa

Show Material materials with Shear modulus of 75.86 GPa

400.0 °C

72 GPa

Show Material materials with Shear modulus of 72 GPa

Unlock all property charts

Tensile strength

20.0 °C

600 MPa

Show Material materials with Tensile strength of 600 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

1.02E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.02E-5 1/K

100.0 °C

1.05E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

200.0 °C

1.09E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.09E-5 1/K

300.0 °C

1.13E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.13E-5 1/K

400.0 °C

1.16E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.16E-5 1/K

500.0 °C

1.2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K

600.0 °C

1.22E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.22E-5 1/K

Unlock all property charts

Max service temperature, long

0 - 550 °C

Show Material materials with Max service temperature, long of 0 - 550 °C

Melting point

1375 - 1450 °C

Show Material materials with Melting point of 1375 - 1450 °C

Typical for Martensitic Stainless Steel

Specific heat capacity

20.0 °C

439 J/(kg·K)

Show Material materials with Specific heat capacity of 439 J/(kg·K)

100.0 °C

474 J/(kg·K)

Show Material materials with Specific heat capacity of 474 J/(kg·K)

200.0 °C

498 J/(kg·K)

Show Material materials with Specific heat capacity of 498 J/(kg·K)

300.0 °C

517 J/(kg·K)

Show Material materials with Specific heat capacity of 517 J/(kg·K)

400.0 °C

538 J/(kg·K)

Show Material materials with Specific heat capacity of 538 J/(kg·K)

500.0 °C

564 J/(kg·K)

Show Material materials with Specific heat capacity of 564 J/(kg·K)

600.0 °C

598 J/(kg·K)

Show Material materials with Specific heat capacity of 598 J/(kg·K)

Unlock all property charts

Thermal conductivity

20.0 °C

25.9 W/(m·K)

Show Material materials with Thermal conductivity of 25.9 W/(m·K)

100.0 °C

25.3 W/(m·K)

Show Material materials with Thermal conductivity of 25.3 W/(m·K)

200.0 °C

25.2 W/(m·K)

Show Material materials with Thermal conductivity of 25.2 W/(m·K)

300.0 °C

25.2 W/(m·K)

Show Material materials with Thermal conductivity of 25.2 W/(m·K)

400.0 °C

25.4 W/(m·K)

Show Material materials with Thermal conductivity of 25.4 W/(m·K)

500.0 °C

25.7 W/(m·K)

Show Material materials with Thermal conductivity of 25.7 W/(m·K)

600.0 °C

25.9 W/(m·K)

Show Material materials with Thermal conductivity of 25.9 W/(m·K)

Unlock all property charts

Thermal diffusivity

20.0 °C

7.6 mm²/s

Show Material materials with Thermal diffusivity of 7.6 mm²/s

100.0 °C

6.6 mm²/s

Show Material materials with Thermal diffusivity of 6.6 mm²/s

200.0 °C

6.1 mm²/s

Show Material materials with Thermal diffusivity of 6.1 mm²/s

300.0 °C

5.8 mm²/s

Show Material materials with Thermal diffusivity of 5.8 mm²/s

400.0 °C

5.3 mm²/s

Show Material materials with Thermal diffusivity of 5.3 mm²/s

500.0 °C

4.8 mm²/s

Show Material materials with Thermal diffusivity of 4.8 mm²/s

600.0 °C

4.1 mm²/s

Show Material materials with Thermal diffusivity of 4.1 mm²/s

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

5.59E-7 Ω·m

Show Material materials with Electrical resistivity of 5.59E-7 Ω·m

100.0 °C

6.4E-7 Ω·m

Show Material materials with Electrical resistivity of 6.4E-7 Ω·m

200.0 °C

7.32E-7 Ω·m

Show Material materials with Electrical resistivity of 7.32E-7 Ω·m

300.0 °C

8.17E-7 Ω·m

Show Material materials with Electrical resistivity of 8.17E-7 Ω·m

400.0 °C

8.97E-7 Ω·m

Show Material materials with Electrical resistivity of 8.97E-7 Ω·m

500.0 °C

9.74E-7 Ω·m

Show Material materials with Electrical resistivity of 9.74E-7 Ω·m

600.0 °C

1.05E-6 Ω·m

Show Material materials with Electrical resistivity of 1.05E-6 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Carbon

0.08 - 0.12 %

Show Material materials with Carbon of 0.08 - 0.12 %

Chromium

12 - 14 %

Show Material materials with Chromium of 12 - 14 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Do you have a technical question or need more information about this material?

Post it as a comment below and receive answers from engineers and other community members.