DIN 17103 Grade StE 420 cold worked, welded and normalized

View all suppliers (2)

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.84 g/cm³

Show Material materials with Density of 7.84 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

-100.0 °C

217 GPa

Show Material materials with Elastic modulus of 217 GPa

20.0 °C

212 GPa

Show Material materials with Elastic modulus of 212 GPa

100.0 °C

207 GPa

Show Material materials with Elastic modulus of 207 GPa

200.0 °C

199 GPa

Show Material materials with Elastic modulus of 199 GPa

300.0 °C

192 GPa

Show Material materials with Elastic modulus of 192 GPa

400.0 °C

184 GPa

Show Material materials with Elastic modulus of 184 GPa

500.0 °C

175 GPa

Show Material materials with Elastic modulus of 175 GPa

600.0 °C

164 GPa

Show Material materials with Elastic modulus of 164 GPa

Elongation

20.0 °C

21 %

Show Material materials with Elongation of 21 %

Elongation, transverse

20.0 °C

19 %

Show Material materials with Elongation, transverse of 19 %

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Low Carbon Steel

Shear modulus

23.0 °C

82 GPa

Show Material materials with Shear modulus of 82 GPa

Typical for Low Carbon Steel

Tensile strength

20.0 °C

530 - 630 MPa

Show Material materials with Tensile strength of 530 - 630 MPa

Tensile strength, transverse

20.0 °C

530 - 630 MPa

Show Material materials with Tensile strength, transverse of 530 - 630 MPa

Yield strength

20.0 °C

375 - 420 MPa

Show Material materials with Yield strength of 375 - 420 MPa

Yield strength, transverse

20.0 °C

375 - 420 MPa

Show Material materials with Yield strength, transverse of 375 - 420 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

-100.0 °C

1.05E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

20.0 °C

1.15E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.15E-5 1/K

100.0 °C

1.21E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.21E-5 1/K

200.0 °C

1.27E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.27E-5 1/K

300.0 °C

1.32E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 1/K

400.0 °C

1.36E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.36E-5 1/K

500.0 °C

1.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.4E-5 1/K

600.0 °C

1.44E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.44E-5 1/K

Unlock all property charts

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

Typical for Low Carbon Steel

Specific heat capacity

-100.0 °C

423 J/(kg·K)

Show Material materials with Specific heat capacity of 423 J/(kg·K)

20.0 °C

461 J/(kg·K)

Show Material materials with Specific heat capacity of 461 J/(kg·K)

100.0 °C

479 J/(kg·K)

Show Material materials with Specific heat capacity of 479 J/(kg·K)

200.0 °C

499 J/(kg·K)

Show Material materials with Specific heat capacity of 499 J/(kg·K)

300.0 °C

517 J/(kg·K)

Show Material materials with Specific heat capacity of 517 J/(kg·K)

400.0 °C

536 J/(kg·K)

Show Material materials with Specific heat capacity of 536 J/(kg·K)

500.0 °C

558 J/(kg·K)

Show Material materials with Specific heat capacity of 558 J/(kg·K)

600.0 °C

587 J/(kg·K)

Show Material materials with Specific heat capacity of 587 J/(kg·K)

Unlock all property charts

Thermal conductivity

-100.0 °C

35.4 W/(m·K)

Show Material materials with Thermal conductivity of 35.4 W/(m·K)

20.0 °C

40.4 W/(m·K)

Show Material materials with Thermal conductivity of 40.4 W/(m·K)

100.0 °C

42 W/(m·K)

Show Material materials with Thermal conductivity of 42 W/(m·K)

200.0 °C

42 W/(m·K)

Show Material materials with Thermal conductivity of 42 W/(m·K)

300.0 °C

40.8 W/(m·K)

Show Material materials with Thermal conductivity of 40.8 W/(m·K)

400.0 °C

38.9 W/(m·K)

Show Material materials with Thermal conductivity of 38.9 W/(m·K)

500.0 °C

36.6 W/(m·K)

Show Material materials with Thermal conductivity of 36.6 W/(m·K)

600.0 °C

34.3 W/(m·K)

Show Material materials with Thermal conductivity of 34.3 W/(m·K)

Unlock all property charts

Thermal diffusivity

-100.0 °C

12.1 mm²/s

Show Material materials with Thermal diffusivity of 12.1 mm²/s

20.0 °C

11.2 mm²/s

Show Material materials with Thermal diffusivity of 11.2 mm²/s

100.0 °C

10.8 mm²/s

Show Material materials with Thermal diffusivity of 10.8 mm²/s

200.0 °C

10.1 mm²/s

Show Material materials with Thermal diffusivity of 10.1 mm²/s

300.0 °C

9.3 mm²/s

Show Material materials with Thermal diffusivity of 9.3 mm²/s

400.0 °C

8.3 mm²/s

Show Material materials with Thermal diffusivity of 8.3 mm²/s

500.0 °C

7 mm²/s

Show Material materials with Thermal diffusivity of 7 mm²/s

600.0 °C

5.8 mm²/s

Show Material materials with Thermal diffusivity of 5.8 mm²/s

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

-100.0 °C

1.93E-7 Ω·m

Show Material materials with Electrical resistivity of 1.93E-7 Ω·m

20.0 °C

2.58E-7 Ω·m

Show Material materials with Electrical resistivity of 2.58E-7 Ω·m

100.0 °C

3.05E-7 Ω·m

Show Material materials with Electrical resistivity of 3.05E-7 Ω·m

200.0 °C

3.76E-7 Ω·m

Show Material materials with Electrical resistivity of 3.76E-7 Ω·m

300.0 °C

4.6E-7 Ω·m

Show Material materials with Electrical resistivity of 4.6E-7 Ω·m

400.0 °C

5.59E-7 Ω·m

Show Material materials with Electrical resistivity of 5.59E-7 Ω·m

500.0 °C

6.75E-7 Ω·m

Show Material materials with Electrical resistivity of 6.75E-7 Ω·m

600.0 °C

8.08E-7 Ω·m

Show Material materials with Electrical resistivity of 8.08E-7 Ω·m

Unlock all property charts

Magnetic

PropertyValueComment

Curie temperature

770 °C

Show Material materials with Curie temperature of 770 °C

Typical for Low Carbon Steel

Chemical properties

PropertyValue

Aluminium

0.02 %

Show Material materials with Aluminium of 0.02 %

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

Chromium

0.3 %

Show Material materials with Chromium of 0.3 %

Copper

0.2 %

Show Material materials with Copper of 0.2 %

Manganese

1 - 1.7 %

Show Material materials with Manganese of 1 - 1.7 %

Molybdenum

0.1 %

Show Material materials with Molybdenum of 0.1 %

Nickel

1 %

Show Material materials with Nickel of 1 %

Niobium

0.05 %

Show Material materials with Niobium of 0.05 %

Nitrogen

0.02 %

Show Material materials with Nitrogen of 0.02 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.1 - 0.6 %

Show Material materials with Silicon of 0.1 - 0.6 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Vanadium

0.2 %

Show Material materials with Vanadium of 0.2 %