General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation, transverse | 20.0 °C | 19 % Show Material materials with Elongation, transverse of 19 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 20.0 °C | 530 - 680 MPa Show Material materials with Tensile strength of 530 - 680 MPa | |
Tensile strength, transverse | 20.0 °C | 530 - 680 MPa Show Material materials with Tensile strength, transverse of 530 - 680 MPa | |
Yield strength | 20.0 °C | 385 MPa Show Material materials with Yield strength of 385 MPa | |
Yield strength, transverse | 20.0 °C | 385 MPa Show Material materials with Yield strength, transverse of 385 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Carbon | 0.23 % Show Material materials with Carbon of 0.23 % |
Manganese | 1 - 1.5 % Show Material materials with Manganese of 1 - 1.5 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 0.55 % Show Material materials with Silicon of 0.55 % |
Sulfur | 0.035 % Show Material materials with Sulfur of 0.035 % |
Do you have a technical question or need more information about this material?