DIN 17172 Grade StE 385.7 TM thermomechanically treated

Want to keep this datasheet? Save it now in your required format

Description

The steel StE 385.7 TM is produced as welded tube in the conditions thermomechanical treated. Tubes of this steel are conform acc. 5L, 5LX and 5LS of the American Petroleum Institute (API). The Attention should be paid to the technical regulation for combustible liquids TRbF 301. Application: pipelines for combustible liquids (e.g. petroleum and his products) and for compressed or liquid combustible gases

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Elongation, transverse

20.0 °C

19 %

Show Material materials with Elongation, transverse of 19 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

20.0 °C

530 - 680 MPa

Show Material materials with Tensile strength of 530 - 680 MPa

Tensile strength, transverse

20.0 °C

530 - 680 MPa

Show Material materials with Tensile strength, transverse of 530 - 680 MPa

Yield strength

20.0 °C

385 MPa

Show Material materials with Yield strength of 385 MPa

Yield strength, transverse

20.0 °C

385 MPa

Show Material materials with Yield strength, transverse of 385 MPa

Chemical properties

PropertyValue

Carbon

0.14 %

Show Material materials with Carbon of 0.14 %

Manganese

1 - 1.6 %

Show Material materials with Manganese of 1 - 1.6 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.45 %

Show Material materials with Silicon of 0.45 %

Sulfur

0.025 %

Show Material materials with Sulfur of 0.025 %