General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation, transverse | 20.0 °C | 18 % Show Material materials with Elongation, transverse of 18 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 20.0 °C | 560 - 710 MPa Show Material materials with Tensile strength of 560 - 710 MPa | |
Tensile strength, transverse | 20.0 °C | 560 - 710 MPa Show Material materials with Tensile strength, transverse of 560 - 710 MPa | |
Yield strength | 20.0 °C | 445 MPa Show Material materials with Yield strength of 445 MPa | |
Yield strength, transverse | 20.0 °C | 445 MPa Show Material materials with Yield strength, transverse of 445 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.16 % Show Material materials with Carbon of 0.16 % |
Manganese | 1 - 1.6 % Show Material materials with Manganese of 1 - 1.6 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 0.55 % Show Material materials with Silicon of 0.55 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |